Marpaung, Petrus Tomu Natal (2023) Pemanfaatan Limbah Cangkang Kerang dan Abu Jerami Sebagai Substitusi Parsial Terhadap Kuat Tekan Beton. S1 thesis, Universitas Kristen Indonesia.
|
Text (Hal_Judul_Daftar_Isi_Abstrak)
HalJudulDaftarIsIAbstrak.pdf Available under License Creative Commons Attribution Non-commercial Share Alike. Download (2MB) |
|
|
Text (BAB_I)
BABI.pdf Available under License Creative Commons Attribution Non-commercial Share Alike. Download (388kB) |
|
|
Text (BAB_II)
BABII.pdf Restricted to Registered users only Available under License Creative Commons Attribution Non-commercial Share Alike. Download (705kB) | Request a copy |
|
|
Text (BAB_III)
BABIII.pdf Restricted to Registered users only Available under License Creative Commons Attribution Non-commercial Share Alike. Download (733kB) | Request a copy |
|
|
Text (BAB_IV)
BABIV.pdf Restricted to Registered users only Available under License Creative Commons Attribution Non-commercial Share Alike. Download (631kB) | Request a copy |
|
|
Text (BAB_V)
BABV.pdf Restricted to Registered users only Available under License Creative Commons Attribution Non-commercial Share Alike. Download (420kB) | Request a copy |
|
|
Text (DAFTAR_PUSTAKA)
DAFTARPUSTAKA.pdf Available under License Creative Commons Attribution Non-commercial Share Alike. Download (415kB) |
|
|
Text (LAMPIRAN)
LAMPIRAN.pdf Restricted to Repository staff only Available under License Creative Commons Attribution Non-commercial Share Alike. Download (1MB) | Request a copy |
Abstract
Penelitian ini menggunakan empat rancangan beton untuk menilai pengaruh dua bahan pengganti. Campuran kontrol memakai pasir dan semen tanpa substitusi. Pada tiga campuran lainnya, cangkang kerang darah menggantikan 10% pasir, sedangkan abu jerami padi menggantikan semen pada kadar 3%, 5%, atau 7%. Rancangan 25 MPa diuji pada silinder berukuran 150 × 300 mm setelah perawatan selama 14 atau 28 hari. Kadar abu 5% menghasilkan rata-rata tertinggi pada kedua umur. Pada hari ke-28, hasilnya 28,21 MPa, lebih tinggi 12,84% daripada kontrol yang mencapai 25,00 MPa. Pada hari ke-14, hasil terendah di antara campuran pengganti tercatat pada kadar abu 3%, yaitu 25,95 MPa. Kata kunci: cangkang kerang darah, abu jerami padi, beton, substitusi parsial, kuat tekan / Four concrete mixtures were prepared to examine how two waste-derived materials affect compressive strength. The reference mixture used sand and cement without replacement. In the other three mixtures, ground blood cockle shells replaced 10% of the sand, while rice straw ash replaced either 3%, 5%, or 7% of the cement. The design strength was 25 MPa. Cylinders measuring 150 × 300 mm were loaded in compression on days 14 and 28. The 5% ash mixture led the tested series at both ages. On day 28, its mean strength was 28.21 MPa, 12.84% above the reference value of 25.00 MPa. On day 14, the weakest of the replacement mixtures was the 3% ash mixture at 25.95 MPa. Keywords: blood cockle shells, rice straw ash, concrete, partial replacement, compressive strength
| Item Type: | Thesis (S1) | ||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Contributors: |
|
||||||||||||
| Subjects: | TECHNOLOGY > Engineering (General). Civil engineering (General) | ||||||||||||
| Divisions: | FAKULTAS TEKNIK > Teknik Sipil | ||||||||||||
| Depositing User: | Mr Petrus Tomu Natal Marpaung | ||||||||||||
| Date Deposited: | 18 Nov 2026 04:52 | ||||||||||||
| Last Modified: | 18 Nov 2026 04:52 | ||||||||||||
| URI: | http://repository.uki.ac.id/id/eprint/24205 |
Actions (login required)
![]() |